Research hydration structure formation of high-temperature gypsum binders on the basis of khujakul deposits

Abstract

The article discusses the processes of high-temperature gypsum binder from the Khujakul deposit of the Republic of Karakalpakstan, in the temperature range of 550-1000°C and simulating the decomposition of its compositions, the phase composition of the resulting products, the main patterns of structure formation are established depending on the phase composition of the original binder.The results of the influence of the concentration of Ca2 on the strength of the structure in concentrated suspensions of gypsum at different temperatures are presented.The ways of regulating the properties of various gypsum binders with the help of additives and rational use of natural gypsum for the production of high-temperature gypsum binder for rocks with a predominance of the clay-carbonate part have been determined.21 As a result of high-temperature firing of carbonate-gypsum mixtures,a binder material with the ability to hydraulic hardening can be obtained.

Other Versions

No versions found

Links

PhilArchive



    Upload a copy of this work     Papers currently archived: 101,072

External links

Setup an account with your affiliations in order to access resources via your University's proxy server

Through your library

  • Only published works are available at libraries.

Similar books and articles

Analytics

Added to PP
2022-09-01

Downloads
4 (#1,803,830)

6 months
2 (#1,685,865)

Historical graph of downloads
How can I increase my downloads?

Citations of this work

No citations found.

Add more citations

References found in this work

No references found.

Add more references